Perusahaan kami bergerak dalam produksi dan perdagangan berbagai jenis baja persegi panjang stainless steel cerah, pipa baja berbentuk khusus berkinerja tinggi, presisi tinggi, dan pipa seamless stainless steel. Kami telah menjalin hubungan bisnis dengan pelanggan di lebih dari 20 negara dan wilayah. Detail seperti metode pembayaran, waktu pengiriman, dan jumlah minimum dapat dinegosiasikan berdasarkan pesanan. Baja karbon: ASTM A105, A350 LF2, LF3, A694 F52, F60, F65, F70
|
Werkstoff‐Nr. |
KERIUHAN. |
AISI. |
UNS. |
AFNOR. | BS. |
JIS |
SS. | gost |
|
1.4000 |
X6Cr13 |
403(410S) |
S 41008 |
Z6C13 |
403 S17 |
SUS 403 |
2301 |
08Bab13 |
|
(X7Cr13) |
||||||||
|
1.4002 |
X6CrAI13 |
405 |
S 40500 |
Z6CAI13 |
405 S17 |
SUS 405 |
‐ |
08Ch11NYU |
|
(X7CrAl13) |
||||||||
|
1.4006 |
X10Cr13 |
410 |
S 41000 |
Z12C13 |
410 S21 |
SUS 410 |
2302 |
12Bab13 |
|
1.4016 |
X6Cr17 |
430 |
S 43000 |
Z8C17 |
430 S15 |
SUS 430 |
2320 |
12Bab17 |
|
(X8CR17) |
430 S17 |
|||||||
|
1.4021 |
X20Cr13 |
420 |
S 42000 |
Z20C13 |
420 S29 |
SUS 420J1 |
2303 |
20Bab13 |
|
420 S37 |
SUS 420J2 |
|||||||
|
420 S45 |
||||||||
|
1.4024 |
X15Cr13 |
410 |
S 41000 |
‐ |
420 S29 |
SUS 410J1 |
‐ |
‐ |
|
410 S21 |
||||||||
|
1.4028 |
X30Cr13 |
420 |
S 42000 |
Z30C13 |
420 S45 |
SUS 420J2 |
2304 |
30Bab13 |
|
1.4031 |
X38Cr13 |
420 |
S 42000 |
Z40C14 |
‐ |
SUS 420J2 |
2304 |
40Bab13 |
|
(X40Cr13) |
||||||||
|
1.4034 |
X46Cr13 |
420 |
S 42000 |
Z40C14 |
420 S45 |
‐ |
‐ |
40Bab13 |
|
Z38C13M |
||||||||
|
1.4057 |
X20CrNi172 |
431 |
S 43100 |
Z15CN16‐02 |
431 S29 |
SUS 431 |
2321 |
20Ch17N2 |
|
(X22CrNi17) |
||||||||
|
1.4510 |
X6CrTi17 |
XM8 |
‐ |
Z8CT17 |
‐ |
SUS 430LX |
‐ |
08Ch17T |
|
(X8CrTi17) |
430Ti |
|||||||
|
1.4512 |
X6CrTi12 |
409 |
S 40900 |
Z6CT12 |
409 S19 |
SUH 409 |
‐ |
‐ |
|
409 S17 |
||||||||
|
1.4301 |
X5CrNi1810 |
304/304H |
S 30400 |
Z6CN18‐09 |
304 S31 |
SUS 304 |
2332 |
08Ch18N10 |
|
(X5CrNi189) |
||||||||
|
1.4305 |
X10CrNiS189 |
303 |
S 30300 |
Z10CNF18‐09 |
303 S21 |
SUS 303 |
2346 |
‐ |
|
(X12CrNiS188) |
||||||||
|
1.4306 |
X2CrNi1911 |
304L |
S 30403 |
Z2CN18‐10 |
304 S12 |
SCS 19 |
2352 |
03Ch18N11 |
|
(X2CrNi189) |
Z3CN19‐10M |
304 C12 |
SUS 304L |
2333 |
||||
|
(G‐X2Cr189) |
Z2CN18‐09 |
304 S11 |
||||||
|
1.4310 |
X12CrNi177 |
301 |
S 30100 |
Z12CN17‐07 |
301 S21 |
SUS301 |
‐ |
‐ |
|
Z12Cn18‐07 |
||||||||
|
1.4311 |
X2CrNiN1810 |
304LN |
S 30453 |
Z2CN18‐10Az |
304 S62 |
SUS 304LN |
2371 |
‐ |
|
1.4401 |
X5CrNiMo17122 |
316 |
S 31600 |
Z6CND17‐11 |
316 S16 |
SUS 316 |
2347 |
‐ |
|
1.4404 |
X2CrNiMo17132 |
316L |
S 31603 |
Z2CND 18‐13 |
316 S14 |
SUS 316L |
2348 |
‐ |
|
(X2CrNiMo1810) |
Z2CND17‐12 |
|||||||
|
(GX2CrNiMo1810) |
||||||||
|
1.4429 |
X2CrNiMoN17133 |
316LN |
S 31653 |
Z2CND17‐13 |
‐ |
SUS 316LN |
2375 |
‐ |
|
(X2CrNiMoN1813) |
||||||||
|
1.4435 |
X2CrNiMo18143 |
316L |
S 31603 |
Z2CND17‐13 |
316 S11 |
SCS 16 |
2353 |
03Ch17N14 |
|
(X2CrNiMo1812) |
316 S12 |
SUS 316L |
M2 |
|||||
|
316 S13 |
||||||||
|
1.4436 |
X5CrNiMo17133 |
316 |
S31600 |
Z6CND17‐12 |
316 S16 |
SUS 316 |
2343 |
‐ |
|
(X5CrNiMo1812) |
316 S33 |
|||||||
|
1.4438 |
X2CrNiMo18164 |
317L |
S 31703 |
Z2CND19‐15 |
317 S12 |
SUS 317L |
2367 |
‐ |
|
(X2CrNiMo1816) |
||||||||
|
1.4439 |
X2CrNiMoN17135 |
317LNM |
S 31726 |
Z2CND19‐15 |
317 S16 |
‐ |
‐ |
‐ |
|
1.4449 |
X5CrNiMo1713 |
317 |
‐ |
‐ |
317 S16 |
SUS 317 |
‐ |
‐ |
|
1.4465 |
X1CrNiMoN25252 |
‐ |
N 08310 |
‐ |
‐ |
‐ |
‐ |
‐ |
|
1.4505 |
X5CrNiMoCuNb2018 |
‐ |
‐ |
‐ |
‐ |
‐ |
‐ |
07Ch17N20 |
|
M2D2T |
||||||||
|
1.4521 |
X2CrMoTi182 |
440 |
S 44400 |
‐ |
‐ |
‐ |
2326 |
‐ |
|
1.4529 |
X1NiCrMoCuN25206 |
‐ |
N08925 |
‐ |
‐ |
‐ |
‐ |
‐ |
|
1.4539 |
X1NiCrMoCu25205 |
904L |
N 08904 |
Z1NCDU25‐ |
‐ |
‐ |
2562 |
‐ |
|
2004 |
||||||||
|
1.4541 |
X6CrNiTi1810 |
321 |
S 32100 |
Z6CNT18‐10 |
321 S12 |
SUS 321 |
2337 |
1Ch18N12T |
|
(X10CrNiTi189) |
321 S20 |
|||||||
|
(321 S31) |
||||||||
|
1.4550 |
X6CrNiNb1810 |
347 |
S 34700 |
Z6CNNb18‐10 |
347 S17 |
SUS 347 |
2338 |
08Ch18N128 |
|
(X10CrNiNb189) |
347 S31 |
|||||||
|
1.4558 |
X2NiCrAlTi3220 |
‐ |
N 08800 |
‐ |
‐ |
‐ |
‐ |
‐ |
|
1.4563 |
X1NiCrMoCuN31274 |
‐ |
N 08028 |
Z1NCDU31273A |
‐ |
‐ |
‐ |
‐ |
|
z |
||||||||
|
1.4571 |
X6CrNiMoTi17122 |
316Ti |
S 31635 |
Z6CNDT17‐12 |
320 S31 |
‐ |
2350 |
10Ch17N13M2T |
|
(X10CrNiMoTi1810) |
320 S17 |
|||||||
|
1.4580 |
X6CrNiMoNb17122 |
316Cb |
‐ |
Z6CNDNb17% e2% 80% 9012 |
‐ |
‐ |
‐ |
08Ch16N13M2B |
|
(X10CrNiMoNb1810) |
Z6CNDNb19‐13 |
|||||||
|
1.4583 |
X10CrNiMoNb1812 |
318 |
‐ |
‐ |
‐ |
‐ |
‐ |
‐ |
|
1.4586 |
X5CrMoCuNb2218 |
‐ |
‐ |
‐ |
‐ |
‐ |
‐ |
‐ |
|
1.4335 |
X1CrNi2521 |
310LC |
‐ |
Z2CN25‐20 |
‐ |
‐ |
‐ |
‐ |
|
1.4713 |
X10CrA17 |
‐ |
‐ |
Z8CA7 |
‐ |
‐ |
‐ |
‐ |
|
1.4718 |
X45CrSi93 |
HNV3 |
‐ |
Z45CS9 |
401 S45 |
SUH1 |
‐ |
‐ |
|
1.4724 |
X10CrAl13 |
(405) |
‐ |
Z10C13 |
403 S17 |
‐ |
‐ |
‐ |
|
1.4742 |
X10CrAl18 |
(430) |
‐ |
Z10CAS18 |
430 S15 |
SUS 430 |
‐ |
‐ |
|
SUH 21 |
||||||||
|
1.4749 |
X18CrN28 |
446‐1 |
‐ |
‐ |
‐ |
‐ |
‐ |
Bab 25 |
|
1.4762 |
X10CrAI24 |
(446) |
‐ |
Z10CAS24 |
‐ |
‐ |
‐ |
‐ |
|
1.4821 |
X20CrNiSi254 |
327 |
‐ |
Z20CNS25‐04 |
‐ |
‐ |
‐ |
‐ |
|
1.4828 |
X15CrNiSi2012 |
309 |
‐ |
Z15CNS20‐12 |
309 S24 |
SUH 309 |
‐ |
Bab 24N12S1 |
|
1.4833 |
X7CrNi2314 |
309S |
‐ |
Z15CN24‐13 |
‐ |
SUS 3095 |
‐ |
‐ |
|
1.4841 |
X15CrNiSi2520 |
314/310 |
‐ |
Z12CNS25‐20 |
‐ |
SUH 310 |
‐ |
20Ch25N20S2 |
|
1.4845 |
X12CrNi2521 |
310 S |
‐ |
Z12CN25‐20 |
310 S24 |
SUH 310 |
2361 |
10Ch23N18 |
|
SUS 310S |
||||||||
|
1.4848 |
(G‐X40CrNiSi2520) |
‐ |
‐ |
‐ |
310 C40 |
SCH 21 |
‐ |
‐ |
|
1.4864 |
X12NiCrSi3616 |
330 |
N 08330 |
Z12NCS37‐18 |
Ya 17 |
SUH 330 |
‐ |
‐ |
|
Z12NCS35‐16 |
||||||||
|
Z12NC37‐18 |
||||||||
|
1.4871 |
X53CrMnNiN219 |
EV8 |
‐ |
Z52CMN21‐09 |
349 S54 |
SH 35 |
‐ |
‐ |
|
SUH 36 |
||||||||
|
1.4876 |
X10NiCrAITi3320 |
B163 |
N 08800 |
Z8NC32‐21 |
NA 15(H) |
NCF |
‐ |
‐ |
|
8000 |
||||||||
|
1.4876 |
X10CrNiAPTi3320 |
B163 |
N 08810 |
Z8NC32‐21 |
TIDAK 15 |
‐ |
‐ |
‐ |
|
1.4878 |
Z12CrNiTi189 |
321H |
‐ |
Z6CNT18‐12(B) |
S21 S20 |
SUS 321 |
2337 |
‐ |
|
(321 S12) |
||||||||
|
1.4893 |
‐ |
‐ |
S 30815 |
‐ |
‐ |
‐ |
2368 |
‐ |
|
‐ |
‐ |
‐ |
S 32750 |
‐ |
‐ |
‐ |
‐ |
‐ |
|
1.4362 |
‐ |
‐ |
S 32304 |
‐ |
‐ |
‐ |
‐ |
‐ |
|
1.4417 |
‐ |
‐ |
S 31500 |
‐ |
‐ |
‐ |
‐ |
‐ |
|
1.4460 |
X4CrNiMo2751 |
329 |
S 32900 |
‐ |
‐ |
SUS |
2324 |
‐ |
|
(XBCrNiMo275) |
329J1 |
|||||||
|
SCH 11 |
||||||||
|
SCH 11 |
||||||||
|
1.4462 |
X2CrNiMoN2253 |
‐ |
S 31803 |
Z2CND22‐05Az |
‐ |
‐ |
‐ |
‐ |
|
‐ |
‐ |
‐ |
S 31200 |
‐ |
‐ |
‐ |
‐ |
‐ |
|
‐ |
‐ |
‐ |
S 31260 |
‐ |
‐ |
‐ |
‐ |
‐ |
|
‐ |
‐ |
‐ |
S 32550 |
‐ |
‐ |
‐ |
‐ |
‐ |
|
‐ |
‐ |
‐ |
S 32950 |
‐ |
‐ |
‐ |
‐ |
‐ |
Perkenalkan Batang Persegi Panjang Stainless Steel
Anda bisa mendapatkan pemahaman yang lebih baik tentangnyaBatang Persegi Panjang Stainless SteelDi Sini.
Batangan datar baja tahan karat 304 dan 316 adalah salah satu produk paling umum yang kami suplai, dengan kualitas lain juga tersedia. Kami menawarkan pemotongan baja datar baja tahan karat dan penggilingan sejati. Jika Anda membutuhkan pengiriman cepat, panjang atau ukuran khusus, silakan hubungi kami. Tim pembelian kami memiliki pengalaman bertahun-tahun untuk memastikan kami menyediakan produk yang paling kompetitif untuk proyek Anda.
Perbedaan antara baja pipih canai asli dan baja pipih yang dicukur atau dipotong dari lembaran adalah toleransi dimensinya. Pada baja pipih sejati, toleransi lebar dan tebal terbatas dan hasil akhirnya lebih baik. Saat memotong batang dari lembaran stok, toleransi diameter lebih longgar dan konsisten dengan metode pemotongan. Potongan baja pipih dari pelat akan memiliki ketebalan yang sama dengan pelat HARP. Toleransi ketebalan pelat cenderung berat. Toleransi minimum bawah untuk ketebalan papan adalah {{0}}0,010", sedangkan toleransi atas tidak terbatas atau setidaknya 0,090" dan meningkat seiring dengan ketebalan.
Batang Persegi Panjang Stainless Steel


Elemen Kimia Batang Persegi Panjang Stainless Steel
| Ukuran | Panjang | Berat (pon/kaki) |
| 1/8" x 1/2" | 144.00" | 0.210 |
| 1/8" x 5/8" | 144.00" | 0.266 |
| 1/8" x 3/4" | 144.00" | 0.319 |
| 1/8" x 1" | 144.00" | 0.425 |
| 1/8" x 1-1/4" | 144.00" | 0.532 |
| 1/8" x 1-1/2" | 144.00" | 0.638 |
| 1/8" x 1-3/4" | 144.00" | 0.744 |
| 1/8" x 2" | 144.00" | 0.850 |
| 1/8" x 2-1/2" | 144.00" | 1.059 |
| 1/8" x 3" | 144.00" | 1.280 |
| 1/8" x 4" | 144.00" | 1.700 |
| 1/8" x 5" | 144.00" | 2.126 |
| 1/8" x 6" | 144.00" | 2.559 |
| 3/16" x 1/2" | 144.00" | 0.319 |
| 3/16" x 3/4" | 144.00" | 0.477 |
| 3/16" x 1" | 144.00" | 0.638 |
| 3/16" x 1-1/4" | 144.00" | 0.797 |
| 3/16" x 1-1/2" | 144.00" | 0.956 |
| 3/16" x 2" | 144.00" | 1.275 |
| 3/16" x 2-1/2" | 144.00" | 1.593 |
Batang Persegi Panjang Stainless Steel


Kimia:
| C | M N | P | S | Ya | Tidak | Kr | Cu | N | Mo |
| .10 Maks | 2.0 Maks | 0,045 Maks | .15-.35 | 1.0 Maks | 8.0-10.0 | 17.0-19.0 | 1.0 Maks | .11 Maks |
Tentang kami
Anda dapat mempelajari lebih lanjut tentang Gnee di sini.
Kunjungan pelanggan asing

Pertanyaan Umum
T: Bisakah saya mendapatkan harga terbaik Anda?
A: Tujuan kami adalah memberi Anda harga terbaik dan jaminan kualitas terbaik dalam jangka panjang. Silakan tinggalkan informasi kontak Anda untuk mendapatkan penawaran terbaik, kami akan memberikan Anda solusi terbaik sesegera mungkin.
Q: Berapa lama waktu pengiriman Anda?
J: Biasanya dibutuhkan waktu 5-10 hari jika barang tersedia. Atau jika barang tidak tersedia, dibutuhkan waktu 15-20 hari, tergantung kuantitasnya.
T: Apakah Anda menyediakan sampel? Apakah gratis atau ekstra?
A: Ya, kami dapat menyediakan sampel gratis tanpa membayar biaya pengiriman.
Q: Tentang Harga Produk Batang Persegi Panjang Stainless Steel?
A:Harga Bervariasi Dari Periode Ke Periode Karena Perubahan Siklus Harga Bahan Baku.
Hubungi kami
Manajer Batang Persegi Panjang Stainless Steel

Tag populer: batang persegi panjang stainless steel, produsen, pemasok, pabrik batang persegi panjang stainless steel Cina, Lingkaran stainless steel, profil terisi baja tahan karat, profil tingkat instalasi stainless steel, profil mesin stainless steel, Persegi panjang stainless steel, profil stainless steel standar